Repair of damage: • Droplet method before clear lacquer application. • After clear lacquer has thoroughly dried, sand surface and re-paint. Spots Points rising up from the paint film. Cause/damage pattern: • Metallic base paint sprayed too dry, so that the metal particles could not incorporate into the Repair of damage: • After the paint surface has dried, lightly sand it with grade P800 sanding paper, clean with Metamerism/color deviations Noticeable when identical color shades undergo a Cause/damage pattern: • Use of paints with pigmentation which was not compatible with the standard, e.g. a green can • Use of an unsuitable mixed or ready made paint to re-tone. Repair of damage: • Repaint using the correct paint. Washing out On paint which has been newly applied but not yet Cause/damage pattern: • Layer too thick, paint not stirred enough. Repair of damage: • Sand and re-paint. Loss of gloss Milky, dreary tarnishing of the paint with more or G468093en 501-36- 24 Paint - General Information 501-36- 24 DESCRIPTION AND OPERATION 201 |